These data come from the manufacturers' websites and datasheets, and have not been verified. Different manufacturers report different data. These tables are not exhaustive. I have provided price in terms of USD per kilogram based on the size closest to 1kg, but many of these filaments do not have a 1kg product.
These data come from the manufacturers' websites and datasheets, and have not been verified. Different manufacturers report different data. These tables are not exhaustive. I have provided price in terms of USD per kilogram based on the size closest to 1kg, but many of these filaments do not have a 1kg product. I really like AtomicFilament, but I sure do wish they would publish more technical specs.


===Polymaker===
===Polymaker===

Revision as of 10:45, 29 November 2024

Keeping notes on various FDM filaments here. The glass transition temperature is ideal for annealling. I've got a Google Sheet now chronicling experience with individual filaments.

Qualitative comparisons

Manufacturers employ additives to change the properties of their filaments, which I don't attempt to address here. Properties may change across different batches of the same filament. These are very rough comparisons based off oral wisdom.

  • Impact strength: ASA > ABS > PC > PETG > PLA
  • Tensile strength: PA >> PC >> ASA > ABS/PETG > PLA
  • UV resistance: ASA > ABS
  • "Chemical" resistance: PETG > ABS
  • Melting temp: PC > ASA > PETG > ABS >> PLA
  • Heat resistance: PC > ASA > ABS > PETG > PLA
  • Printing speed:
  • Offensiveness (odor, VOCs while printing): ABS > ASA, PA, PC
  • Acetone postprocessing: ASA/ABS only
  • Ease of sanding: PLA > PETG > ABS/ASA
  • Ease of painting: PLA > PETG > ABS/ASA
  • Tendency to warp: PC > ABS/ASA > PLA > PETG
  • Hygroscopicity: PA/TPU > PETG/ABS/ASA > PLA
  • Filament density: PETG/PLA > ABS/ASA
  • Hotend temp required: PC > ABS/ASA > PETG > PLA

Tables

These data come from the manufacturers' websites and datasheets, and have not been verified. Different manufacturers report different data. These tables are not exhaustive. I have provided price in terms of USD per kilogram based on the size closest to 1kg, but many of these filaments do not have a 1kg product. I really like AtomicFilament, but I sure do wish they would publish more technical specs.

Polymaker

Filament Density (g/cm³) Glass transition (℃) Vicat softening (℃) Heat deflection (℃) Young's modulus XY (MPa) Young's modulus Z (MPa) Tensile strength XY (MPa) Tensile strength Z (MPa) Bending modulus XY (MPa) Charpy XY (kJ/m²) MSRP ($/kg)
PC-ABS 1.1 109 135 112 1835 1677 40 23 2081 26 49.99
PolyMax PC 1.19 113 117 114 2436 2150 53 41 2050 21 51.99
PolyMax PC-FR 1.2 115 116 110 2634 2743 67 46 2518 11.7 54.99
Polymaker PC-PBT 1.2 140 139 107 1849 1659 43 29 1934 21 54.99
Fiberon PET-CF17 1.34 79 238 148 5481 3559 66 28 4744 5 49.98
Fiberon PA6-GF25 1.2 70 191 4431 3330 85 61 4637 17 59.98
Fiberon PPS-CF10 1.29 98 268 253 5314 2790 36 32 4647 5 139.98
PolyLite PC 1.19 113 120 111 2497 2371 69 53 2640 4 29.99
Fiberon PA6-CF20 1.17 74 215 7454 4355 105 68 8339 13 79.98
Fiberon PA12-CF10 1.06 55 131 3304 1801 72 43 3535 13 139.98

Bambu

Parameter Print temp (℃) Print speed (mm/s) Filament density (g/cm³) Tensile strength (MPa) Breaking elongation rate Bending modulus (MPa) Bending strength (MPa) Impact strength (kJ/m²) Melt index (g/10min) Melting temp (℃ ) Heat deflection temp (℃ ) Vicat softening temp (℃) Flow rate ratio Foaming rate Vol. expansion ratio Print density (g/cm³)
PLA Aero 210 - 260 <180 1.21 24 ± 2 2.6 ± 0.7 1690 ± 120 45 ± 4 28.8 ± 1.3 7.7 ± 0.6 153 53 54 0.5-0.8 0-120 100 - 220 0.55 - 1.05
ASA 240 - 270 <250 1.05 37 ± 3 9.2 ± 1.4 1920 ± 130 65 ± 5 41.0 ± 2.3 7.0 ± 0.8 210 100 106 0.93-0.97 n/a 102 1.03
ASA Aero 240 - 280 <150 0.99 32 ± 4 5.1 ± 1.6 1510 ± 120 58 ± 6 32.0 ± 2.5 1.56 ± 0.5 204 85 80 0.45-0.80 0-110 100 - 210 0.46 - 0.97
PC 250 - 270 <300 1.2 55 ± 4 3.8 ± 0.3 2310 ± 70 108 ± 4 34.8 ± 2.1 32.2 ± 2.9 228 117 119
ABS 240 - 270 <300 1.05 33 ± 3 10.5 ± 1.0 1880 ± 110 62 ± 4 39 ± 3.6 34.2 ± 3.8 200 87 94
ABS-GF 240 - 270 <180 1.08 36 ± 3 6.3 ± 1.2 2860 ± 130 68 ± 4 14.5 ± 1.5 7.56 ± 1.4 202 99 103
PETG-Trans 230 - 260 <220 1.25 33 ± 4 8.2 ± 1.3 1610 ± 130 68 ± 3 37.4 ± 3.3 11.7 ± 1.5 228 74 79
PETG-HF 230 - 260 <300 1.28 34 ± 4 8.6 ± 1.2 2050 ± 120 64 ± 3 31.5 ± 2.2 28.2 ± 2.7 214 69 70
PA6-CF 260 - 290 <100 1.09 102 ± 7 5.8 ± 1.6 5460 ± 280 151 ± 8 40.3 ± 2.5 6.8 ± 0.6 223 186 212
PPA-CF 280 - 310 <100 1.25 168 ± 4 3.2 ± 0.4 9860 ± 480 208 ± 6 41.7 ± 2.8 8.4 ± 0.7 258 227 232
PLA-CF 210 - 240 <200 1.22 38 ± 4 8.4 ± 3.2 3950 ± 190 89 ± 4 23.2 ± 3.7 3.7 ± 0.6 165 55 69
PPS-CF 310 - 340 <100 1.26 87 ± 5 1.2 ± 0.4 7160 ± 280 142 ± 5 27.8 ± 2.3 11.48 ± 1.23 284 264 268
PAHT-CF 260 - 290 <100 1.06 92 ± 7 8.4 ± 1.8 4230 ± 210 125 ± 7 57.5 ± 3.4 14.4 ± 2.0 225 194 220
ASA-CF 250 - 280 <250 1.02 34 ± 3 9.6 ± 1.4 3740 ± 130 72 ± 5 14.0 ± 2.2 1.74 ± 0.3 210 110 108
PA6-GF 260 - 290 <130 1.14 75 ± 6 3.9 ± 0.8 3670 ± 140 120 ± 6 27.7 ± 2.2 9.0 ± 0.8 219 182 210